Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Round Bars 19Cr 36Co 25Ni 7.0Mo 0.50Cb 2.9Ti 0.20Al 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened and Aged, Modified Strength ( Reaffirmed: Aug 2007 )
standard by SAE International, 04/01/2003
Description
This specification covers a corrosion and heat-resistant, work strengthened and aged cobalt-nickel-chromium alloy in the form of bars 2 inches (50.8 mm) and under in nominal diameter.These bars have been used typically for parts, such as fasteners, requiring a room temperature minimum tensile strength of 170 ksi (1172 MPa) for use up to 850 \mDF (454 \mDC) in applications requiring high ductility to promote toughness and resistance to cracking under shock loading conditions, but usage is not limited to such applications. This alloy exhibits exceptionally good resistance to corrosion, crevice corrosion, and stress-corrosion cracking.
Product Details
- Published:
- 04/01/2003
- File Size:
- 1 file , 160 KB
- Note:
- This product is unavailable in Ukraine, Russia, Belarus